Ihowuliseleli China Fused Ceramic Foundry Sand for 3D Printing
Ngobuchwepheshe obuphezulu kunye nezixhobo, ulawulo olungqongqo oluphezulu, ixabiso elifanelekileyo, inkampani ekhethekileyo kunye nentsebenziswano esondeleyo kunye nethemba, sizinikele ekunikezeni awona maxabiso angcono kubathengi bethu kwi-Wholesale yase-China Fused Ceramic Foundry Sand yoShicilelo lwe-3D, ngokufudumeleyo. wamkelekile ukusebenzisana kunye nokuphuhlisa nathi! siya kuqhubeka nokubonelela ngemveliso enomgangatho ophezulu kunye nexabiso elikhuphisanayo.
Ngobuchwephesha obuphezulu kunye nezixhobo, ulawulo olungqongqo oluphezulu, ixabiso elifanelekileyo, inkampani ekhethekileyo kunye nentsebenziswano esondeleyo kunye nethemba, sizinikele ekunikezeni ixabiso elingcono kakhulu kubathengi bethu, iminyaka emininzi, ngoku sibambelele kwi umgaqo ojolise kubathengi, usekwe kumgangatho, ukulandela ukugqwesa, ukwabelana ngenzuzo efanayo. Siyathemba, ngokunyaniseka okukhulu nangentando elungileyo, ukuba newonga lokunceda kwimarike yakho eyongezelelweyo.
Iimbonakalo
• Ukwakhiwa kwecandelo elifanayo
• Ubungakanani bokutya okuzinzileyo kunye nokungena komoya
• Ukuchasa okuphezulu (1825°C)
• Ukuchasana okuphezulu kokugqoka, ukutyumza kunye nokutshatyalaliswa kwe-thermal
• Ukwandiswa kwe-thermal encinci
• Ubumanzi obugqwesileyo kunye nokusebenza kakuhle kokuzalisa ngenxa yokuba singqukuva
• Elona nqanaba liphezulu lokulungiswa kwakhona kwisixokelelwano se-santi loop
Iinkqubo zeSicelo seSand Foundry
Inkqubo yesanti efakwe kwi-resin
Ibhokisi ebandayo kunye nenkqubo yesanti yebhokisi efudumeleyo
Inkqubo yoshicilelo lwesanti ye-3D
Inkqubo yesanti ye-resin yokungabhaki (Bandakanya i-Furan resin kunye ne-Alkali phenolic resin)
Inkqubo yotyalo-mali/ Inkqubo yokufunyanwa kwewax elahlekileyo/Ukwenziwa ngokuchanekileyo
Inkqubo yobunzima obulahlekileyo/ Inkqubo yogwebu elahlekileyo
Inkqubo yeglasi yamanzi
Ipropati yeSanti yeCeramic
ICandelo leMichiza eliPhambili | Al₂O₃ 70-75%, Fe₂O₃<4%, |
Imilo yeenkozo | I-Spherical |
I-Angular Coefficient | ≤1.1 |
Ubungakanani obuyinxenye | 45μm -2000μm |
Ukuchasa | ≥1800℃ |
Unizi lolwapho kuyiwa khona | 1.8-2.1 g/cm3 |
PH | 6.5-7.5 |
Isicelo | Intsimbi, intsimbi, intsimbi |
Ukwabiwa kobungakanani beenkozo
Umnatha | 20 | 30 | 40 | 50 | 70 | 100 | 140 | 200 | 270 | Ipani | Uluhlu lwe-AFS |
μm | 850 | 600 | 425 | 300 | 212 | 150 | 106 | 75 | 53 | Ipani | |
#400 | ≤5 | 15-35 | 35-65 | 10-25 | ≤8 | ≤2 | 40±5 | ||||
#500 | ≤5 | 0-15 | 25-40 | 25-45 | 10-20 | ≤10 | ≤5 | 50±5 | |||
#550 | ≤10 | 20-40 | 25-45 | 15-35 | ≤10 | ≤5 | 55±5 | ||||
#650 | ≤10 | 10-30 | 30-50 | 15-35 | 0-20 | ≤5 | ≤2 | 65±5 | |||
#750 | ≤10 | 5-30 | 25-50 | 20-40 | ≤10 | ≤5 | ≤2 | 75±5 | |||
#850 | ≤5 | 10-30 | 25-50 | 10-25 | ≤20 | ≤5 | ≤2 | 85±5 | |||
#950 | ≤2 | 10-25 | 10-25 | 35-60 | 10-25 | ≤10 | ≤2 | 95±5 |
Ngobuchwepheshe obuphezulu kunye nezixhobo, ulawulo olungqongqo oluphezulu, ixabiso elifanelekileyo, inkampani ekhethekileyo kunye nentsebenziswano esondeleyo kunye nethemba, sizinikele ekunikezeni awona maxabiso angcono kubathengi bethu kwi-Wholesale yase-China Fused Ceramic Foundry Sand yoShicilelo lwe-3D, ngokufudumeleyo. wamkelekile ukusebenzisana kunye nokuphuhlisa nathi! siya kuqhubeka nokubonelela ngemveliso enomgangatho ophezulu kunye nexabiso elikhuphisanayo.
Ihoseyili , Kwiminyaka emininzi, ngoku sibambelele kumgaqo ojolise kubathengi, usekwe kumgangatho, ukulandela ukugqwesa, ukwabelana ngenzuzo efanayo. Siyathemba, ngokunyaniseka okukhulu nangentando elungileyo, ukuba newonga lokunceda kwimarike yakho eyongezelelweyo.